Oxidized Bitumen

Description

Oxidized bitumen is blown from blowing hot air to pure bitumen at the final stage of the purification operation in this process, hot air with a temperature of 200 to 300 degrees Celsius is blown through a perforated tube into a compartment containing bitumen.
Oxidized bitumen is categorized based on softening points and penetration rate. For example, oxidized bitumen 85/40 is a type of bitumen whose softening point is 85±5 degrees Centigrade and its penetration rate is 40±5 (0.1mm). Oxidized bitumen is also expected to make up for weight loss under heat. The softening point in oxidized bitumen is much higher than in regular bitumen, causing lower thermal sensitivity.

Packing

Various pickings are available for customer’s purposes and conveniences:

  • Kraft bag
  • Meltable plastic bag
  • Drum
  • Bulk
Properties

This process gives the Oxidized Bitumen more rubbery properties than its original formula and they are simply harder bitumen.

Uses of OXIDIZED Bitumen
  • Oxidized bitumen is used for the repair and sealing of joints or cracks.
  • Oxidized bitumen is used as an adhesive to be used in thermal insulation.
  • Oxidized bitumen is used in various industries like roofing, isolation, insulation flooring, mastics, pipe coatings, and electrical applications.

Oxidized Bitumen Products:

OXIDIZED BITUMEN 85-25

Oxidized Bitumen 85/25

BINDER PROPERTIES REQUIREMENTS TEST METHOD
MIN MAX
Density@25°C 1.05 approx. ASTM D70
penetration @25°C 20 30 ASTM D5
Softening point, °C 80 90 ASTM D36
Flash point, °C 250 - ASTM D92
Solubility in trichloroethylene, % 99.0 - ASTM D2042
Spot test, xylene Negative AASHTO T102
Test on residue After TFOT
Change of Mass WT% - 0.2 ASTM D6
OXIDIZED BITUMEN 90-15

Oxidized Bitumen 90/15

BINDER PROPERTIES REQUIREMENTS TEST METHOD
MIN MAX
Density@25°C 1.05 approx. ASTM D70
penetration @25°C 10 20 ASTM D5
Softening point, °C 85 95 ASTM D36
Flash point, °C 250 - ASTM D92
Solubility in trichloroethylene, % 99.0 - ASTM D2042
Spot test, xylene Negative AASHTO T102
Test on residue After TFOT
Change of Mass WT% - 0.2 ASTM D6
OXIDIZED BITUMEN 95-15

Oxidized Bitumen 95/15

BINDER PROPERTIES REQUIREMENTS TEST METHOD
MIN MAX
Density@25°C 1.05 approx. ASTM D70
penetration @25°C 10 20 ASTM D5
Softening point, °C 90 100 ASTM D36
Ductility @ 25°C 1.5 - ASTM D113
Flash point, °C 250 - ASTM D92
Solubility in trichloroethylene, % 99.0 - ASTM D2042
Spot test, xylene Negative AASHTO T102
Test on residue After TFOT
Change of Mass WT% - 0.2 ASTM D6
OXIDIZED BITUMEN 95-25

Oxidized Bitumen 95/25

BINDER PROPERTIES REQUIREMENTS TEST METHOD
MIN MAX
Density@25°C 1.05 approx. ASTM D70
penetration @25°C 20 30 ASTM D5
Softening point, °C 90 100 ASTM D36
Flash point, °C 250 - ASTM D92
Solubility in trichloroethylene, % 99.0 - ASTM D2042
Spot test, xylene Negative AASHTO T102
Test on residue After TFOT
Change of Mass WT% - 0.2 ASTM D6
OXIDIZED BITUMEN 115-15

Oxidized Bitumen 115/15

BINDER PROPERTIES REQUIREMENTS TEST METHOD
MIN MAX
Density@25°C 1.05 approx. ASTM D70
penetration @25°C 10 20 ASTM D5
Softening point, °C 110 120 ASTM D36
Ductility @ 25°C 1.5 - ASTM D113
Flash point, °C 250 - ASTM D92
Solubility in trichloroethylene, % 99.0 - ASTM D2042
Spot test, xylene Negative AASHTO T102
Test on residue After TFOT
Change of Mass WT% - 0.2 ASTM D6
OXIDIZED BITUMEN 125-10

Oxidized Bitumen 125/10

BINDER PROPERTIES REQUIREMENTS TEST METHOD
MIN MAX
Density@25°C 1.05 approx. ASTM D70
penetration @25°C 7 12 ASTM D5
Softening point, °C 120 130 ASTM D36
Flash point, °C 250 - ASTM D92
Solubility in trichloroethylene, % 99.0 - ASTM D2042
Spot test, xylene Negative AASHTO T102
Test on residue After TFOT
Change of Mass WT% - 0.2 ASTM D6