Penetration Bitumen

Description

Penetration Bitumen is a Semi-Hard Black material known as Petroleum Grade Bitumen. Asphalt Penetration Bitumen is produced by blowing hot air into the vacuum bottom. Penetration Grade Bitumen is mainly used in road surfacing. Bitumen with a Lower Penetration Grade is used in regions with Warm climates, while a Higher Penetration Grade is used in Cold weather.

Packing
  • 180(Kg) new steel drum.
  • 220(Liter) new steel drum.
  • Jumbo Bag 1000(kg), 300(kg) and 250(kg).
Application

Penetration bitumen has a wide range of applications in the construction industry, including:

  1. Road construction: Penetration bitumen is extensively used in the construction of asphalt pavements for roads, highways, and airports. It is applied as a binder between aggregate materials to form a strong and durable surface.
  2. Roofing: Penetration bitumen is also used in the construction of roofs, where it is applied as a waterproofing material. It is typically used in built-up roofing systems, which are composed of several layers of bitumen and reinforcing materials.
  3. Waterproofing: Penetration bitumen is used to waterproof a variety of structures, including bridges, tunnels, and retaining walls. It can be applied as a coating or as a component of a waterproofing system.
  4. Industrial applications: Penetration bitumen is used in various industrial applications, such as pipeline coating, corrosion protection, and insulation.

Overall, penetration bitumen is a versatile material that provides excellent adhesion, durability, and resistance to deformation. It is a critical component in many construction projects and plays a vital role in ensuring the longevity and safety of structures.

Penetration Bitumen Products:

Penetration Bitumen 40/50

Penetration Bitumen 40/50

BINDER PROPERTIES REQUIREMENTS TEST METHOD
MIN MAX
Density@25°C 1010 1060 ASTM D70
penetration @25°C 40 50 ASTM D5
Softening point, °C 52 60 ASTM D36
Ductility @ 25°C 100 - ASTM D113
Flash point, °C 250 - ASTM D92
Solubility in trichloroethylene, % 99.0 - ASTM D2042
Spot test, xylene, Negative AASHTO T102
Test on residue After TFOT
Change of Mass WT% - 0.2 ASTM D6
Drop in Penetration% - 20 ASTM D6-D5
Penetration Bitumen 50/70

Penetration Bitumen 50/70

BINDER PROPERTIES REQUIREMENTS TEST METHOD
MIN MAX
Density@25°C 1010 1060 ASTM D70
penetration @25°C 50 70 ASTM D5
Softening point, °C 46 56 ASTM D36
Ductility @ 25°C 100 - ASTM D113
Flash point, °C 250 - ASTM D92
Solubility in trichloroethylene, % 99.0 - ASTM D2042
Spot test, xylene, Negative AASHTO T102
Test on residue After TFOT
Change of Mass WT% - 0.2 ASTM D6
Drop in Penetration% - 20 ASTM D6-D5
Penetration Bitumen 60/70

Penetration Bitumen 60/70

BINDER PROPERTIES REQUIREMENTS TEST METHOD
MIN MAX
Density@25°C 1010 1060 ASTM D70
penetration @25°C 60 70 ASTM D5
Softening point, °C 49 56 ASTM D36
Ductility @ 25°C 100 - ASTM D113
Flash point, °C 250 - ASTM D92
Solubility in trichloroethylene, % 99.0 - ASTM D2042
Spot test, xylene, Negative AASHTO T102
Test on residue After TFOT
Change of Mass WT% - 0.2 ASTM D6
Drop in Penetration% - 20 ASTM D6-D5
Penetration Bitumen 70/100

Penetration Bitumen 70/100

BINDER PROPERTIES REQUIREMENTS TEST METHOD
MIN MAX
Density@25°C 1010 1060 ASTM D70
penetration @25°C 70 100 ASTM D5
Softening point, °C 45 52 ASTM D36
Ductility @ 25°C 100 - ASTM D113
Flash point, °C 250 - ASTM D92
Solubility in trichloroethylene, % 99.0 - ASTM D2042
Spot test, xylene, Negative AASHTO T102
Test on residue After TFOT
Change of Mass WT% - 0.2 ASTM D6
Drop in Penetration% - 20 ASTM D6-D5
Penetration Bitumen 85/100

Penetration Bitumen 85/100

BINDER PROPERTIES REQUIREMENTS TEST METHOD
MIN MAX
Density@25°C 1010 1060 ASTM D70
penetration @25°C 85 100 ASTM D5
Softening point, °C 42 - ASTM D36
Ductility @ 25°C 100 - ASTM D113
Flash point, °C 250 - ASTM D92
Solubility in trichloroethylene, % 99.0 - ASTM D2042
Spot test, xylene, Negative AASHTO T102
Test on residue After TFOT
Change of Mass WT% - 0.2 ASTM D6
Drop in Penetration% - 20 ASTM D6-D5
Penetration Bitumen 100/120

Penetration Bitumen 100/120

BINDER PROPERTIES REQUIREMENTS TEST METHOD
MIN MAX
Density@25°C 1010 1060 ASTM D70
penetration @25°C 100 120 ASTM D5
Softening point, °C 42 49 ASTM D36
Ductility @ 25°C 100 - ASTM D113
Flash point, °C 250 - ASTM D92
Solubility in trichloroethylene, % 99.0 - ASTM D2042
Spot test, xylene, Negative AASHTO T102
Test on residue After TFOT
Change of Mass WT% - 0.2 ASTM D6
Drop in Penetration% - 20 ASTM D6-D5
Penetration Bitumen 120/150

Penetration Bitumen 120/150

BINDER PROPERTIES REQUIREMENTS TEST METHOD
MIN MAX
Density@25°C 1010 1060 ASTM D70
penetration @25°C 120 150 ASTM D5
Softening point, °C 38 - ASTM D36
Ductility @ 25°C 100 - ASTM D113
Flash point, °C 218 - ASTM D92
Solubility in trichloroethylene, % 99.0 - ASTM D2042
Spot test, xylene, Negative AASHTO T102
Test on residue After TFOT
Change of Mass WT% - 0.2 ASTM D6
Drop in Penetration% - 20 ASTM D6-D5
Penetration Bitumen 150/200

Penetration Bitumen 150/200

BINDER PROPERTIES REQUIREMENTS TEST METHOD
MIN MAX
Density@25°C 1010 1060 ASTM D70
penetration @25°C 150 200 ASTM D5
Softening point, °C 36 - ASTM D36
Ductility @ 25°C 100 - ASTM D113
Flash point, °C 218 - ASTM D92
Solubility in trichloroethylene, % 99.0 - ASTM D2042
Spot test, xylene, Negative AASHTO T102
Test on residue After TFOT
Change of Mass WT% - 0.2 ASTM D6
Drop in Penetration% - 20 ASTM D6-D5