Description
Penetration Bitumen is a Semi-Hard Black material known as Petroleum Grade Bitumen. Asphalt Penetration Bitumen is produced by blowing hot air into the vacuum bottom. Penetration Grade Bitumen is mainly used in road surfacing. Bitumen with a Lower Penetration Grade is used in regions with Warm climates, while a Higher Penetration Grade is used in Cold weather.
- 180(Kg) new steel drum.
- 220(Liter) new steel drum.
- Jumbo Bag 1000(kg), 300(kg) and 250(kg).
Penetration bitumen has a wide range of applications in the construction industry, including:
- Road construction: Penetration bitumen is extensively used in the construction of asphalt pavements for roads, highways, and airports. It is applied as a binder between aggregate materials to form a strong and durable surface.
- Roofing: Penetration bitumen is also used in the construction of roofs, where it is applied as a waterproofing material. It is typically used in built-up roofing systems, which are composed of several layers of bitumen and reinforcing materials.
- Waterproofing: Penetration bitumen is used to waterproof a variety of structures, including bridges, tunnels, and retaining walls. It can be applied as a coating or as a component of a waterproofing system.
- Industrial applications: Penetration bitumen is used in various industrial applications, such as pipeline coating, corrosion protection, and insulation.
Overall, penetration bitumen is a versatile material that provides excellent adhesion, durability, and resistance to deformation. It is a critical component in many construction projects and plays a vital role in ensuring the longevity and safety of structures.
Penetration Bitumen Products:
Penetration Bitumen 40/50
Penetration Bitumen 40/50
|
BINDER PROPERTIES |
REQUIREMENTS |
TEST METHOD |
|
MIN |
MAX |
|
Density@25°C |
1010 |
1060 |
ASTM D70 |
|
penetration @25°C |
40 |
50 |
ASTM
D5 |
|
Softening point, °C |
52 |
60 |
ASTM
D36 |
|
Ductility @ 25°C |
100 |
- |
ASTM
D113 |
|
Flash point, °C |
250 |
- |
ASTM
D92 |
|
Solubility in trichloroethylene, % |
99.0 |
- |
ASTM
D2042 |
|
Spot test,
xylene, |
Negative |
AASHTO
T102 |
|
Test on residue After TFOT |
|
Change of
Mass WT% |
- |
0.2 |
ASTM D6 |
|
Drop in Penetration% |
- |
20 |
ASTM
D6-D5 |
Penetration Bitumen 50/70
Penetration Bitumen 50/70
|
BINDER PROPERTIES |
REQUIREMENTS |
TEST METHOD |
|
MIN |
MAX |
|
Density@25°C |
1010 |
1060 |
ASTM D70 |
|
penetration @25°C |
50 |
70 |
ASTM
D5 |
|
Softening point, °C |
46 |
56 |
ASTM
D36 |
|
Ductility @ 25°C |
100 |
- |
ASTM
D113 |
|
Flash point, °C |
250 |
- |
ASTM
D92 |
|
Solubility in trichloroethylene, % |
99.0 |
- |
ASTM
D2042 |
|
Spot test, xylene, |
Negative |
AASHTO
T102 |
|
Test on residue After TFOT |
|
Change of
Mass WT% |
- |
0.2 |
ASTM D6 |
|
Drop in Penetration% |
- |
20 |
ASTM
D6-D5 |
Penetration Bitumen 60/70
Penetration Bitumen 60/70
|
BINDER PROPERTIES |
REQUIREMENTS |
TEST METHOD |
|
MIN |
MAX |
|
Density@25°C |
1010 |
1060 |
ASTM D70 |
|
penetration @25°C |
60 |
70 |
ASTM
D5 |
|
Softening point, °C |
49 |
56 |
ASTM
D36 |
|
Ductility @ 25°C |
100 |
- |
ASTM
D113 |
|
Flash point, °C |
250 |
- |
ASTM
D92 |
|
Solubility in trichloroethylene, % |
99.0 |
- |
ASTM
D2042 |
|
Spot test, xylene, |
Negative |
AASHTO
T102 |
|
Test on residue After TFOT |
|
Change of
Mass WT% |
- |
0.2 |
ASTM D6 |
|
Drop in Penetration% |
- |
20 |
ASTM
D6-D5 |
Penetration Bitumen 70/100
Penetration Bitumen 70/100
|
BINDER PROPERTIES |
REQUIREMENTS |
TEST METHOD |
|
MIN |
MAX |
|
Density@25°C |
1010 |
1060 |
ASTM D70 |
|
penetration @25°C |
70 |
100 |
ASTM
D5 |
|
Softening point, °C |
45 |
52 |
ASTM
D36 |
|
Ductility @ 25°C |
100 |
- |
ASTM
D113 |
|
Flash point, °C |
250 |
- |
ASTM
D92 |
|
Solubility in trichloroethylene, % |
99.0 |
- |
ASTM
D2042 |
|
Spot test, xylene, |
Negative |
AASHTO
T102 |
|
Test on residue After TFOT |
|
Change of
Mass WT% |
- |
0.2 |
ASTM D6 |
|
Drop in Penetration% |
- |
20 |
ASTM
D6-D5 |
Penetration Bitumen 85/100
Penetration Bitumen 85/100
|
BINDER PROPERTIES |
REQUIREMENTS |
TEST METHOD |
|
MIN |
MAX |
|
Density@25°C |
1010 |
1060 |
ASTM D70 |
|
penetration @25°C |
85 |
100 |
ASTM
D5 |
|
Softening point, °C |
42 |
- |
ASTM
D36 |
|
Ductility @ 25°C |
100 |
- |
ASTM
D113 |
|
Flash point, °C |
250 |
- |
ASTM
D92 |
|
Solubility in trichloroethylene, % |
99.0 |
- |
ASTM
D2042 |
|
Spot test, xylene, |
Negative |
AASHTO
T102 |
|
Test on residue After TFOT |
|
Change of
Mass WT% |
- |
0.2 |
ASTM D6 |
|
Drop in Penetration% |
- |
20 |
ASTM
D6-D5 |
Penetration Bitumen 100/120
Penetration Bitumen 100/120
|
BINDER PROPERTIES |
REQUIREMENTS |
TEST METHOD |
|
MIN |
MAX |
|
Density@25°C |
1010 |
1060 |
ASTM D70 |
|
penetration @25°C |
100 |
120 |
ASTM
D5 |
|
Softening point, °C |
42 |
49 |
ASTM
D36 |
|
Ductility @ 25°C |
100 |
- |
ASTM
D113 |
|
Flash point, °C |
250 |
- |
ASTM
D92 |
|
Solubility in trichloroethylene, % |
99.0 |
- |
ASTM
D2042 |
|
Spot test, xylene, |
Negative |
AASHTO
T102 |
|
Test on residue After TFOT |
|
Change of
Mass WT% |
- |
0.2 |
ASTM D6 |
|
Drop in Penetration% |
- |
20 |
ASTM
D6-D5 |
Penetration Bitumen 120/150
Penetration Bitumen 120/150
|
BINDER PROPERTIES |
REQUIREMENTS |
TEST METHOD |
|
MIN |
MAX |
|
Density@25°C |
1010 |
1060 |
ASTM D70 |
|
penetration @25°C |
120 |
150 |
ASTM
D5 |
|
Softening point, °C |
38 |
- |
ASTM
D36 |
|
Ductility @ 25°C |
100 |
- |
ASTM
D113 |
|
Flash point, °C |
218 |
- |
ASTM
D92 |
|
Solubility in trichloroethylene, % |
99.0 |
- |
ASTM
D2042 |
|
Spot test, xylene, |
Negative |
AASHTO
T102 |
|
Test on residue After TFOT |
|
Change of
Mass WT% |
- |
0.2 |
ASTM D6 |
|
Drop in Penetration% |
- |
20 |
ASTM
D6-D5 |
Penetration Bitumen 150/200
Penetration Bitumen 150/200
|
BINDER PROPERTIES |
REQUIREMENTS |
TEST METHOD |
|
MIN |
MAX |
|
Density@25°C |
1010 |
1060 |
ASTM D70 |
|
penetration @25°C |
150 |
200 |
ASTM
D5 |
|
Softening point, °C |
36 |
- |
ASTM
D36 |
|
Ductility @ 25°C |
100 |
- |
ASTM
D113 |
|
Flash point, °C |
218 |
- |
ASTM
D92 |
|
Solubility in trichloroethylene, % |
99.0 |
- |
ASTM
D2042 |
|
Spot test, xylene, |
Negative |
AASHTO
T102 |
|
Test on residue After TFOT |
|
Change of
Mass WT% |
- |
0.2 |
ASTM D6 |
|
Drop in Penetration% |
- |
20 |
ASTM
D6-D5 |